MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Hilox ™ 961 Mac-A960S Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: A high quality alumina ceramic of 96% Al2O3 content. Excellent mechanical characteristics make this an ideal material for components where resistance to dynamic wear and abrasive action are prime factors.

Prime Features:

  • Exceptionally hard-wearing
  • Excellent abrasion resistance
  • High compressive and flexural strengths
  • Dense, non-porous and vacuum tight
  • Excellent dimensional stability across very wide temperature range
  • Resists chemical attack
Typical Applications:
  • Valve plates for liquid and gas control systems: industrial and domestic duties
  • Pneumatic slider valves (>20 million operating cycles can be achieved)
  • Wear resistant components for rotary and reciprocating pumps: shafts, bearings, thrust washers, plungers, counterface seats, etc
Production Capabilities:
  • Complex components to close tolerances
  • Exacting flatness and surface finishes for low friction valve operation and accurate flow control.
  • Flatness tolerance below three helium bnads (0.0009 mm)
  • Flat surface polished finish to 0.08 micron Ra
  • Cylindrical surface finish to 0.2 micron Ra
  • Prototype, batch and volume prodcution

Information provided by Morgan Advanced Materials

Key Words: Mac-A960S
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.88 g/ccfired
Open Porosity 0.00 %fully dense, % nominal, apparent
Grain Size 2.8 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell HR45N 84
Modulus of Elasticity 354 GPa
@Temperature 20.0 °C
Young's
Flexural Strength 376 MPa
@Temperature 20.0 °C
3-point
Compressive Strength 2100 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+6 ohm-cm
@Temperature 600 °C
 >= 1.00e+8 ohm-cm
@Temperature 300 °C
 >= 1.00e+14 ohm-cm
@Temperature 20.0 °C
Dielectric Constant 10
@Frequency 1e+6 Hz
Dielectric Strength 28.0 kV/mm
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.20 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.880 J/g-°C
Thermal Conductivity 21.0 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 1500 °Cno load
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 96 %
 
Descriptive Properties
Colorbrown
Thermal Downshock160 sC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF5002 / 200240

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.