MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) Alperform® UV A 0018-04 ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Acrylonitrile/Butadiene/Styrene/Copolymer. Filler/additive system: light stabilizer. For use in Acrylonitrile/Butadiene/Styrene/Copolymer. Special Features: dust-free, high dispersibility. Application: building and construction, sport and leisure, injection molded parts, extruded parts, blow molded parts

Information provided by ALBIS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 160 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm3/10min, volumetric value; ISO 1133
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °Cinjection molding
Mold Temperature 50.0 - 80.0 °Cinjection molding
Drying Temperature 80.0 °C
@Time 10800 - 21600 sec
in air circulating dryer, dependant on moisture content
 80.0 °C
@Time 7200 - 14400 sec
in desiccant dryer, depends on moisture content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical AF342F ABS, Flame Retardant, High Flow
Kingfa HF-606 Flame Retardant ABS
Trinseo EMERGE™ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer

PALBIS9907 / 221003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.