MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • ASTM D1056-07 2A1 grade material
  • Fine cell-manufactured in blocks (buns)
  • Approved source for Delphi SD2-207, paragraph 6.10
  • Widely used, low density pure EPDM material
  • ASTM D6576-07 Type II, Grades B & C, Condition Soft

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.00 - 5.00 lb/ft³ASTM D1056
Water Absorption <= 10 %ASTM D1056
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 30 - 40ASTM D2240
Tensile Strength 40.0 psiASTM D412, Die A
Elongation at Break 175 %ASTM D412, Die A
Compressive Strength 2.00 - 5.00 psi
@Strain 25 %
ASTM D1056
Resilience 45[%]; ASTM D2632
Tear Strength >= 6.80 pliDie C; ASTM D624
Compression Set <= 40 %ASTM D1056
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 220 °FContinuous; ASTM D746
 250 °FIntermittent; ASTM D746
Minimum Service Temperature, Air -70.0 °FASTM D746
 
Descriptive Properties
Accelerated Aging±30%Change in Compression Deflection, 7 days at 70°C, ASTM D1056
ColorBlack
FlammabilityFMVSS302Pass at >4.76 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Armacell Monarch® F-03092 (Black) EPDM Foam
Armacell Ensolite™ ECF-400 EPDM crushed foam
Armacell Monarch® F-08001 (Black) Pure EPDM Foam
Armacell Ensolite™ EF0 EPDM crushed foam

PARMD090 / 186701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.