MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Baystar™ HL 428 HDPE Film Grade, Film Properties
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Characteristics:

  • Excellent processability
  • Good tear and impact strength
  • Good stiffness
  • Excellent compatibility with LDPE and LLDPE
  • Excellent drawdown

Applications:

  • Multi-wall liners
  • Gas flush poultry bags
  • Mailing envelopes
  • Heavy-duty shipping sacks
  • Fresh cut produce packaging
  • Coextruded films

Film tested was produced at 1.0 mil with a 2.5:1 BUR

Information provided by Bayport Polymers LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.947 g/cc0.0342 lb/in³ASTM D-792
Water Vapor Transmission 10.9 g/m²/day
@Temperature 37.8 °C
0.700 g/100 in²/day
@Temperature 100 °F
ASTM F1249
Thickness 25.4 microns1.00 milAs Tested
Melt Flow 0.23 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.23 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
High Load Melt Index 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 23.4 MPa3400 psiASTM D-882, A
Film Tensile Strength at Yield, TD 26.2 MPa3800 psiASTM D-882, A
Film Elongation at Break, MD 450 %450 %ASTM D-882, A
Film Elongation at Break, TD 600 %600 %ASTM D-882, A
Elmendorf Tear Strength MD 10 g10 gASTM D1922
Elmendorf Tear Strength TD 1450 g1450 gASTM D1922
Dart Drop Test <= 50.0 g<= 0.110 lbASTM D1709, A
Film Tensile Strength at Break, MD 62.1 MPa9000 psiASTM D-882, A
Film Tensile Strength at Break, TD 18.6 MPa2700 psiASTM D-882, A
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C267 °FASTM D-3417
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
Blow-up Ratio (BUR) 2.52.5As Tested
 
Descriptive Properties
FLH/D6:1as tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBAYST816 / 251112

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.