MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ 2227ED Metallocene Polyethylene Resin (European Grade)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Exceed 2227ED is a metallocene ethylene-hexene copolymer. It offers an excellent balance of high modulus and impact strength. The higher melt index makes it ideally suited for LDPE rich blends

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: 750 ppm
  • Slip: 1250 ppm
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Bread Bags
  • Freezer Film
  • Hygiene Film
  • Overwrap Film
  • Packaging Films

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccExxonMobil method
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 750 ppm
Slip Level 1250 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 540 %ASTM D882
Film Elongation at Break, TD 620 %ASTM D882
Elmendorf Tear Strength MD 230 gASTM D1922
Elmendorf Tear Strength TD 450 gASTM D1922
Dart Drop Test 150 gASTM D1709
Film Tensile Strength at Break, MD 5800 psiASTM D882
Film Tensile Strength at Break, TD 5400 psiASTM D882
1% Secant Modulus, MD 49000 psiASTM D882
1% Secant Modulus, TD 48000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 253 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 6.0 %ASTM D1003
Gloss 12 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force11 lbfExxonMobil Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Enable™ 35-05HH Metallocene Polyethylene Resin (European Grade)
ExxonMobil ACHIEVE 3825 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications
ExxonMobil Enable™ 40-02HH Metallocene Polyethylene Resin
ExxonMobil Escorene® LD 701.ID Blown Film Resin

PEX99054 / 175290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.