EUDRAGIT S 12,5 are anionic copolymers based on methacrylic acic and methyl methacrylate. Physical properties: It is a colorless and clear to slightly cloudy liquid with the characteristic odour of isopropyl alcohol. Characteristics: - Granulation of drug substances in powder form for controlled release
- Effective and stable enteric coatings with a fast dissolution in the upper Bowel
- Site specific drug delivery in intestine by combination with EUDRAGIT S grades
- Variable release profiles
CAS number: 25086 – 15 – 1Chemical/ IUPAC name: Poly(methacrylic acid-co-methyl methacrylate) 1:2 INCI name: Acrylates Copolymer Information provided by Evonik |