MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nucrel® 407 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: 4 wt% Methacrylic Acid.

Nucrel® 0407 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins.

Features/Benefits vs. PE: Better adhesion to unprimed foil, paper and metallized film provides better substrate protection for improved structure reliability and barrier integrity. This product provides good adhesion to PE. Lower seal initiation temperature allows higher speed packaging. Better hot tack, sealability through contamination and heat seal strength provides stronger, more reliable heat seals.

Typical Applications: Foil-containing shampoo, toothpaste, towelette, condiment and miscellaneous non-food pouches and sachets. Snack structures. Other foil, metallized film, or paper coatings as a heat seal or tie layer.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hot Tack Strength 800 g/25 mmseal bar 110°C; Packforsk method.
 
Thermal PropertiesOriginal ValueComments
Melting Point 84.0 °CFreezing Point via DSC/ASTM D3418
 109 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 90.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 305 °CTypical Die Temp.
Melt Temperature 260 - 315 °Cflat die equipment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
Dow Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
Dow Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film

PDUPJ1 / 33635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.