MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EF378 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: WESTLAKE EF378 is suggested for cast film applications. It has excellent haze and gloss, good strength, good processability, and good heat sealability.

    Application/Uses
  • Diaper liners
  • General purpose clarity

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Excellent haze and gloss, good strength, good processability, and good heat sealability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/ccASTM D1505
Thickness 1.25 mil
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 350 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Dart Drop 80.0 g/milASTM D1709
Film Tensile Strength at Break, MD 3500 psiASTM D882
Film Tensile Strength at Break, TD 2700 psiASTM D882
1% Secant Modulus, MD 25000 psiASTM D882
1% Secant Modulus, TD 29000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 5.5 %ASTM D1003
Gloss 70 %at 45º; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 390 °Fwith BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Blow Molding Applications)
Geon® Performance Solutions Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid
Braskem FT200WV Homopolymer Polypropylene
Braskem 5D49 Polypropylene Homopolymer
Braskem 52T30V Homopolymer Polypropylene

PWESF056 / 84493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.