MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Konson CaO-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% Finely selected calcium oxide, 20% EPDM binder and dispersing agents

Use Characteristics: Konson® CaO-80 is a desiccant provided in EPDM rubber predispersed granules. Normal CaO binds the moisture by the formation of calcium hydroxide (Ca(HO)2). The enables the production of vulcanizates to be cured without pressure and which, otherwise, even in using vacuum extruders, show porosity due to the moisture still present in the compounds. This is why Konson®CaO-80 is preferably used in extrusion compounds which have to be cured continuously either in open hot air, fluid beds, salt baths or in the UHF equipment. Konson® CaO-80 and also be recommended for the use in expanded compounds, particularly in microcellular sponge, because Konson® CaO-80 provides a more uniform cell structure.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective CaO is assured.

Dosage levels: The normal dosage is between 2 and 10 phr. It is mainly determined by the expected moisture content which mostly depends on the amount and type of filler used.

Applications: Automotive and construction profile sealants, belts, straps, conveyor belts, rollers, cable coverings, rubber floorings.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.25 g/cc0.0813 lb/in³
 
Descriptive Properties
AppearanceGrey-white granules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS024 / 256069

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.