MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMW® 73 Copper Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and wear resistance is obtained in both cast and wrought material largely by means of heat treatment. It is generally useful where high stress is encountered or where high abrasion resistance is desired but where temperatures are not excessive. The annealing temperature is somewhat less than for other heat treatable high strength copper base alloys. The hardness of CMW® 73 material in the fully heat treated condition is sufficiently high to make machining somewhat difficult particularly in drilling and tapping of small holes. Where extensive machining or forming is to be done, CMW® 73 material can be supplied in the solution annealed (soft) condition and then hardened by a simple heat treatment following machining.

CMW® 73 material is useful where extremely high hardness, strength and abrasion resistance is required. It may be advantageously used for certain flash and projection welding dies where high mechanical properties are required but where current density and heat are not excessive. Many of the steel strip flash welders in continuous steel strip mills are equipped with CMW® 73 die facings. The high hardness and abrasion resistance of CMW® 73 material makes it ideally suited for current carrying collets, chucks, bearings and shafts. Current carrying structural members of CMW® 73 material provide extremely high strength.

Information provided by CMW Inc.

1

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 38Rod & Bar
 38Casting
 38Forging
Tensile Strength, Ultimate 758 MPaCastings
 1170 MPaBar, Rod & Forgings
Tensile Strength, Yield 589 MPaCastings
 1030 MPaBar, Rod & Forgings
Elongation at Break 2.0 %Castings
 4.0 %Rod & bar
 6.0 %Forging
Modulus of Elasticity 128 GPa
Fatigue Strength 165 MPacasting
 207 MPaForging
 241 MPaRod & Bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000750 ohm-cmForgings (23 % IACS)
 0.00000780 ohm-cmDrawn Rod & Bar (22% IACS)
 0.00000860 ohm-cmCastings (20 % IACS)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.8 µm/m-°C
@Temperature 100 °C
Thermal Conductivity 130 W/m-K
Melting Point 857 - 982 °C
Solidus 857 °C
Liquidus 982 °C
Softening Point 375 °CPermanent Softening
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.9 %
Co + Ni 0.40 %
Copper, Cu 97.7 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eagle Brass 151 ZHC® COPPER, 3/4 Hard
Cadi MOLD-MOR™ 3
Bohler-Uddeholm BeCu Alloy 172 Mold Material
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00)
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)

NCMW070 / 15883

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.