MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Americhem Engineered Compounds ColorRx™ ABS-0502AF Food Grade ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: A high gloss, injection molding grade of ABS with FDA food contact approval, containing antimicrobial protection.

All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.

Key Words: ABS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 in/inASTM D955
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 6900 psiASTM D638
Elongation at Break 26 %ASTM D638
Flexural Modulus 380000 psiASTM D790
Izod Impact, Notched 4.00 ft-lb/in
@Temperature 22.8 °C
0.125"; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 183 °FUnannealed (0.5"); ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ebbtide Polymers 972 Transparent ABS, Food Contact Grade
INEOS Styrolution Lustran® 248FC Acrylonitrile Butadiene Styrene (ABS)
Ineos ABS Lustran® 1148 General Purpose, High-Impact
Aclo Accucomp ABS ABS801V Automotive Approved Grade
PTS Trilac® TR558-CL ABS- Transparent ABS

PLTLC069 / 104454

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.