Notes: Monprene CP-35124 X1 is a general purpose clear thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-35124 X1 is a low hardness grade suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Low Density; Lubricated; Low Specific Gravity; Low Hardness; Medium Flow; Slip; Without Fillers Uses: Consumer Applications; Gaskets; Handles; kitchenware; Sporting Goods; Toothbrush Handles; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Preliminary data. Information provided by Teknor Apex |