MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Compounds HM-372A (Comp) LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: Key Features
  • UL component recognition listing (E141240), UL-94 V2 flame rating
  • Good moldability
  • Balance of toughness and rigidity
  • Good low temperature impact
  • Compounded for uniform additive dispersion
  • Standard, custom or special effect colors available
  • Also available in powder form as HMP-372A
Availability: North America

Features: Good Moldability; Good Toughness; High Rigidity; Ignition Resistant; Low Temperature Impact Resistance

UL File Number: E141240

Appearance: Colors Available

Form: Pellets

Processing Method: Compression Molding

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³Base Resin; ASTM D792
 1.01 g/cc0.0365 lb/in³Base Compound; ASTM D792
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.3 MPa2800 psiCompression Molded; ASTM D638
Elongation at Break 300 %300 %Compression Molded; ASTM D638
Flexural Modulus 0.724 GPa105 ksiTangent, Compression Molded; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94  V-2
@Thickness 1.52 mm
V-2
@Thickness 0.0600 in
 V-2
@Thickness 3.30 mm
V-2
@Thickness 0.130 in
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 - 22.0 min0.250 - 0.367 hourStart-up: 18 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAVAGO41212 / 311905

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.