MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® S 5228 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® S 5228 is a food grade, gelular, weakly basic anion exchange resin based on a crosslinked polyacrylate of a special bead size distribution. Due to its acrylic structure, Lewatit S 5228 is able to adsorb and desorb naturally occurring organic substances very effectively. Its high total capacity, its outstanding mechanical stability and its excellent resistance to osmotic shock make it unique for all demineralization applications. Lewatit S 5228 is particularly suitable for the following applications:
  • the demineralization of aqueous solutions such as gelatin, fruit juices, whey and food acids operated with co-current or modern counter-current systems like e.g. Lewatit WS System
  • the removal of organic matter
If using Lewatit S 5228 to treat potable water and the aqueous solutions listed above, special care should be given to the initial cycles of the new resin.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.680 g/cc0.0246 lb/in³
Density 1.07 g/cc0.0387 lb/in³
Bead Size 0.500 - 0.600 mm0.0197 - 0.0236 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 40.0 °C104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceIvory-colored, translucent
pH Operating Range0 - 8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8830 / 209222

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.