MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aurora Plastics GPP1001V0M-HCO-15 PP
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: A medium flow polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high level of flame retardancy.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 - 1.00 g/ccASTM D1505
Melt Flow 12 - 18 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 2700 psiASTM D638
Elongation at Break >= 100 %ASTM D638
Flexural Modulus >= 135000 psiASTM D790-79
Izod Impact, Notched >= 0.750 ft-lb/inASTM D256
Dart Drop, Total Energy >= 15.0 ft-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Flammability Test 5.0
Oxygen Index >= 28 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aurora Plastics GPP1001V0M-HCO PP
PolyMirae Moplen EP500M Injection Molding Grade Polypropylene
PolyMirae Moplen EP300L Injection Molding Grade Polypropylene
LyondellBasell Pro-fax SB786 Polypropylene Impact Copolymer
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant

PSEPO054 / 141017

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.