MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
AK Steel 304L Austenitic Stainless steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive conditions. It often eliminates the necessity of annealing weldments except for applications specifying stress relief. It has slightly lower mechanical properties than Type 304.

Information provided by AK Steel

Key Words: UNS S30403
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.03 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80
Tensile Strength, Ultimate 586 MPa
Tensile Strength, Yield 241 MPa
@Strain 0.2 %
Elongation at Break 55 %in 2 inches
Tensile Modulus 193 GPa
Poissons Ratio 0.24Calculated
Shear Modulus 78.0 GPatorsion
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
 0.000116 ohm-cm
@Temperature 659 °C
Magnetic Permeability <= 1.02H = 200 Oersted, Annealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.9 µm/m-°C
@Temperature 0.000 - 100 °C
 18.7 µm/m-°C
@Temperature <=649 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 16.2 W/m-K
@Temperature 100 °C
 21.4 W/m-K
@Temperature 500 °C
Melting Point 1399 - 1454 °C
Solidus 1399 °C
Liquidus 1454 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 18 - 20 %
Iron, Fe 65.045 - 74 %As Remainder
Manganese, Mn <= 2.0 %
Nickel, Ni 8.0 - 12 %
Nitrogen, N <= 0.10 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 304L Stainless Steel
AISI Type 304L Stainless Steel, Annealed Bar, Longitudinal
304 Stainless Steel
FloMet 304L Stainless Steel
Eagle Brass 304L Austenitic Stainless Steel, Annealed

NAKS108 / 14711

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.