MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® US 2350 Two-Component Flexible, Flame Retardant, Polyurethane Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Loctite Stycast US 2350 provides the following product characteristics:

Cure: Room temperature cure

Application: Potting and Encapsulating

Typical Assembly Applications: Circuit Board Protection, Automotive electronic applications or Telecommunication devices

Loctite Stycast US 2350 is a flexible, flame retardant, mineral filled, polyurethane compound. This potting compound has long pot life, and is low viscosity so it flows well and adheres to many substrates. It has very low odor and does not contain TDI or mercury compounds.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccPart A
 1.40 g/ccCured
 1.46 g/ccPart B
Water Absorption 0.090 %
@Time 86400 sec
Brookfield Viscosity 55 cPRVF, Spindle 2, speed 20 rpm
 2400 cPMixed; RVF, Spindle 2, speed 20 rpm
 13000 cPRVF, Spindle 5, speed 20 rpm
Linear Mold Shrinkage 0.0085 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
Tensile Strength 3.28 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.12e+13 ohm-cm
Surface Resistance 1.54e+15 ohm
Dielectric Constant 4.09
@Frequency 100000 Hz
 5.06
@Frequency 1000 Hz
 6.14
@Frequency 100 Hz
Dielectric Strength 954 V/mil
@Thickness 20.0 mm
Dissipation Factor 0.042
@Frequency 100000 Hz
 0.132
@Frequency 1000 Hz
 0.178
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.510 W/m-K
Flammability, UL94 V-2
@Thickness 6.10 mm
 V-0
@Thickness 9.53 mm
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 3.00 hour
@Temperature 65.0 - 85.0 °C
Alternate
 12.0 - 24.0 hour
@Temperature 23.0 °C
Recommended
Working Life 45.0 min
@Temperature 25.0 °C
300 g
Gel Time 90.0 min300 gram mass
 103 minTechne Gel, 140 gram mass
 
Descriptive Properties
AppearanceBlackCured
 BlackPart B
 BrownPart A
Mix Ratio, by Volume1 : 4Part A : Part B
Mix Ratio, by Weight21 : 100Component A : Component B
Weight Loss (%)0.19Weight Loss after 168 hrs @ 125ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7967 / 255451

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.