3M™ Adhesion Promoter N200NT is a liquid primer used to improve the adhesion of 3M™ Acrylic Foam and Acrylic Plus Tapes to Polyvinyl Chloride (PVC), Polyurethane (PU) and SUS. Since formulations and surface energies vary for these materials, each application should be verified through testing. 3M Adhesion Promoter N200NT is specifically formulated to be used with 3M Acrylic Foam and Acrylic Plus Tapes for automotive applications. 3M Adhesion Promoter N200NT has also been formulated to significantly reduce the hazardous air pollutant (HAPS) content as compared to 3M™ Adhesion Promoter N200J.Information provided by 3M |