TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electronic, appliance, automotive and optical industries. Characteristics: - Medium viscosity
- Self Extinguishing
Applications: All information provided by Samyang |