MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem PRB 0131 RACO Random Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low haze, and excellent impact strength. Its applications include: high transparency thermoformed packaging for food, cosmetics, hygiene, and cleaning products; bottles for food, cosmetics, and cleaning products; returnable water bottles; and high transparency sheets, toy kits, and cosmetic packages.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM-D792
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 79ASTM-D785
Tensile Strength, Yield 28.0 MPaASTM-D638
Elongation at Yield 13 %ASTM-D638
Flexural Modulus, 1% Secant 900 MPaASTM-D790
Izod Impact, Notched 300 J/mASTM-D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °CASTM-D648
Vicat Softening Point 130 °C
@Load 1.02 kg
ASTM-D1525
 
Optical PropertiesOriginal ValueComments
Haze 24 %
@Thickness 1.00 mm
ASTM-D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem PRA 0852 RACO Random Polypropylene Copolymer
Braskem Prisma 2910 RACO Random Polypropylene Copolymer
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene
Braskem Prisma 2400 RACO Random Polypropylene Copolymer

PBRAS939 / 106785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.