MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Special Metals INCONEL® alloy 22 Austenitic Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperatures. This alloy provides exceptional resistance to general corrosion, pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. Alloy 22 has found numerous applications in the chemical/petrochemical processing, pollution control (flue gas desulfurization), power, marine, pulp and paper processing, and waste disposal industries.

Information Provided by Special Metals Corporation

Key Words: UNS N06022; W. Nr. 2.4602; NiCr21Mo14W; ASTM B462; ASTM B564; ASTME SB 564; ASTM B 574; ASME 2226; N-621; ISO 9723; 9724; DIN 17752; 17753; 17754; ASTM B 575; B906; DIN 17750; ISO 6208; ASTM B 619; ASTM B 622; DIN 17751; ASTM B 366; DIN 17744
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.61 g/cc0.311 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8989Plate
 8989Bar
 9393Sheet
Tensile Strength at Break 772 MPa112000 psiPlate
 793 MPa115000 psiBar
 841 MPa122000 psiSheet
Tensile Strength, Yield  365 MPa
@Strain 0.2 %
52900 psi
@Strain 0.2 %
Plate
 379 MPa
@Strain 0.2 %
55000 psi
@Strain 0.2 %
Bar
 434 MPa
@Strain 0.2 %
62900 psi
@Strain 0.2 %
Sheet
Elongation at Break 54 %54 %Sheet
 60 %60 %Bar
 62 %62 %Plate
Modulus of Elasticity 209 GPa30300 ksiDynamic
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0001215 ohm-cm0.0001215 ohm-cm
Magnetic Permeability <= 1.001<= 1.001at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.42 µm/m-°C
@Temperature 193 °C
6.900 µin/in-°F
@Temperature 379 °F
Specific Heat Capacity 0.381 J/g-°C0.0911 BTU/lb-°F
Thermal Conductivity  7.3995 W/m-K
@Temperature 23.0 °C
51.353 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
 10.148 W/m-K
@Temperature 100 °C
70.427 BTU-in/hr-ft²-°F
@Temperature 212 °F
 14.089 W/m-K
@Temperature 300 °C
97.778 BTU-in/hr-ft²-°F
@Temperature 572 °F
 16.4 W/m-K
@Temperature 500 °C
114 BTU-in/hr-ft²-°F
@Temperature 932 °F
 22.733 W/m-K
@Temperature 700 °C
157.77 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 23.696 W/m-K
@Temperature 900 °C
164.45 BTU-in/hr-ft²-°F
@Temperature 1650 °F
 27.56 W/m-K
@Temperature 1100 °C
191.3 BTU-in/hr-ft²-°F
@Temperature 2010 °F
Melting Point 1351 - 1387 °C2464 - 2529 °F
Solidus 1351 °C2464 °F
Liquidus 1387 °C2529 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.015 %<= 0.015 %
Chromium, Cr 20 - 22.5 %20 - 22.5 %
Cobalt, Co <= 2.5 %<= 2.5 %
Iron, Fe 2.0 - 6.0 %2.0 - 6.0 %
Manganese, Mn <= 0.50 %<= 0.50 %
Molybdenum, Mo 12.5 - 14.5 %12.5 - 14.5 %
Nickel, Ni 50.015 - 63 %50.015 - 63 %Balance
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si <= 0.080 %<= 0.080 %
Sulfur, S <= 0.020 %<= 0.020 %
Tungsten, W 2.5 - 3.5 %2.5 - 3.5 %
Vanadium, V <= 0.35 %<= 0.35 %
 
Descriptive Properties
Critical Crevice Temperature (°C)75
Critical Pitting Temperature (°C)>85

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® Alloy 600
Special Metals INCONEL® Alloy C-276
Special Metals INCONEL® Alloy HX
Special Metals INCONEL® Alloy 617
Special Metals INCONEL® Alloy 625

NINDA06 / 98897

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.