MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of complexity and near full theoretical density by utilizing Metal Injection Molding (MIM).  MIM can economically produce complex shapes beyond the capability of conventional Powdered Metallurgy.
    Benefits of Metal Injection Molding
  • 96-98% of Theoretical Density
  • Excellent Mechanical Properties
  • Avoids Costly Secondary Operations
  • Excellent Surface Finishes
  • Capable of Extreme 3-D Geometries
  • Holds Tight Tolerances
  • Extremely Thin Wall Section Capabilities

Information Provided by PolyAlloys, a division of PSM Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.60 g/cc0.275 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 4545Macro
Tensile Strength, Ultimate >= 255 MPa>= 37000 psi
 290 MPa42000 psiTypical
Tensile Strength, Yield  >= 110 MPa
@Strain 0.2 %
>= 16000 psi
@Strain 0.2 %
 124 MPa
@Strain 0.2 %
18000 psi
@Strain 0.2 %
Elongation at Yield >= 20 %>= 20 %in 1 in.
 40 %40 %in 1 in.; Typical
Modulus of Elasticity 193 GPa28000 ksi
Charpy Impact, Unnotched 136 J100 ft-lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel
PSM Industries PolyAlloys MIM-2700 sintered Low Alloy Steel
Kinetics MIM 2.5% SiFe Soft Magnetic Steel
Kinetics MIM F1537 (ASTM F1537) HIP and Heat Treat
Kinetics MIM K3 Heat Treat as Sintered

NPSM001 / 93192

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.