MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
HB Fuller EY3010 Epoxy
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Two part, thixotropic epoxy compounds designed for use with Shur-Lok fasteners to achieve high strength and dependable bonded inserts in honeycomb panels. The handling properties of these products are similar. However, EY3010 is designed for lowest weight. EY3010 is available within NASA limits for low Volatile content required for space application. EY3010 A/B is qualified to LAC 30-8036A.

Features and Benefits:

  • Excellent Sag Resistance Even Through Powder Coating Processes
  • Extremely Light Weight
  • Self Extinguishing
  • Excellent Bonding to Metals, Composites, Coatings, and Most Plastics
  • Excellent Chemical Resistance
  • Excellent Thermal Performance
  • Meets NASA limits for Low Volatile Content Required for Space Applications
  • Room Temperature Cure

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.580 g/cc
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 11.0 MPaOverlap, Aluminum, Acid Etched; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.80 W/m-KASTM E1461
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour
@Temperature 66.0 °C
Full Cure
 168 hour
@Temperature 23.0 °C
Full Cure
Gel Time 20.0 - 25.0 min
Shelf Life 12.0 Month
 
Descriptive Properties
ColorLight Blue
ConsistencyThixotropic Liquid
Mix Ratio100 to 8Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL109 / 316900

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.