MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ETEC (EnvisionTEC) ETEC E-ToughFlex DLP 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: With E-ToughFlex resin, you can produce extremely strong parts, with nearly four times the impact resistance as most engineering plastics. Compatible 3D printing systems for this material are those based Processed by DMSL on continuous digital light processing technology (cDLM) such as Envision One cDLM Mechanical or Envision One cDLM HT. E-ToughFlex™ has a very high flexural modulus and strength and it is hydrophobic (water repellence). Parts 3D printed with E-ToughFlex are strong, yet flexible and have a beautiful surface finish similar to ceramic while having a great abrasion resistance.

Applications:

  • Consumer Goods
  • Manufacturing
  • Medical devices
  • Education

Information provided by Proto3000

Key Words: Digital Light Processing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 660 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 18.0
Hardness, Shore D 89.0 - 90.0
Tensile Strength, Ultimate 67.5 MPa
 68.9 MPa
@Temperature -37.0 °C,
Time 173000 sec
after immersion in water
Elongation at Break 16.0 %
 14.0 %
@Temperature -37.0 °C,
Time 173000 sec
after immersion in water
Modulus of Elasticity 1.34 GPa
 1.33 GPa
@Temperature -37.0 °C,
Time 173000 sec
after immersion in water
Flexural Strength 120 MPaUltimate, after immersion in water
 136 MPaUltimate
Flexural Modulus 3660 MPa
 3300 MPa
@Temperature -37.0 °C,
Time 173000 sec
after immersion in water
Izod Impact, Notched 20.0 J/m
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROTO804 / 322817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.