MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
OCTAL DPET™/PE Lock-Up Laminate Sheet
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging.

Information provided by OCTAL Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission <= 2.00 g/m²/day
@Temperature 23.0 °C
50% RH; ASTM F1249
Oxygen Transmission Rate <= 20.0 cc/m²/day23°C; 50% RH; ASTM F1927
Viscosity Measurement >= 0.74Intrinsic; ASTM D3835
Thickness 270 - 750 micronsincludes both PET and PE layers
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 50.0 MPaASTM D882
Tear Strength >= 0.270 kg(f)/cmBond strength between laminate layers; ASTM F88F88M
Seal Strength >= 3330 g/25 mmUsing OCTAL Lidding Film; ASTM F88F88M
 
Optical PropertiesOriginal ValueComments
Haze <= 10 %ASTM D1003
Transmission, Visible >= 88 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 121 - 154 °CThermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GrafTech EN Envelope Edge-Seal
Aluminum 1050-H18
Aluminum 3105-H26
Aluminum 1050-O
Aluminum 1050-H16

POCTAL995 / 133505

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.