Telcar TL-3050-88 RED is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. It is a high durometer, high tensile strength grade that is RoHS compliant. This grade is UL listed and is suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: General Purpose; Good Colorability; Good Flexibility; Good Melt Strength; Halogen Free; High Elasticity; High Elongation; High Hardness; Low Flow; High Specific Gravity Uses: Connectors; Electrical Parts; General Purpose; Grommets; Insulation; Strain Reliefs; Weatherstripping; Wet Rated Insulation; Wire & Cable Applications Agency Rating: UL 1581 RoHS Compliant:RoHS UL File Number: QMFZ2.E54709 Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |