MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion BrushForm® 158 Copper-Nickel-Tin Cold Rolled Strip (UNS C72900), HT (TS04)
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: BrushForm® 158 Strip is a high-performance, heat treated spinodal copper nickel tin alloy designed to provide optimal formability and strength characteristics in conductive spring applications such as electronic connectors, switches, and sensors.

Information supplied by Materion.

Key Words: ASTM B740
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 370 - 450
Tensile Strength, Ultimate 1205 - 1415 MPa
Tensile Strength, Yield 1170 - 1380 MPa
@Strain 0.2 %
Elongation at Break 1.0 %
@Thickness >=0.100 mm
Modulus of Elasticity 144 GPa
Poissons Ratio 0.30
Shear Modulus 55.4 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000250 ohm-cm
Magnetic Permeability <= 1.01
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.4 µm/m-°C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 76 - 78 %As Balance
Nickel, Ni 14.5 - 15.5 %
Tin, Sn 7.5 - 8.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion BrushForm® 158 Copper-Nickel-Tin Cold Rolled Strip (UNS C72900), 1/4HT (TS01)
Materion BrushForm® 158 Copper-Nickel-Tin Cold Rolled Strip (UNS C72900), AT(TX00)
Materion AuSn Plus Modified Gold-Tin Solder
Materion BrushForm® 158 Copper-Nickel-Tin Cold Rolled Strip (UNS C72900), 1/2HT (TS02)
Materion BrushForm® 158 Copper-Nickel-Tin Cold Rolled Strip (UNS C72900), EHT (TS08)

NBB63436 / 192291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.