MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 2550 FC PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Ultradur B 2550 FC is an unfilled, easy flow PBT offering good heat resistance. This grade is a food contact grade.

Applications: Applications include monofilament, bristles and heat-resistant coatings on paper and board used for packaging frozen foods and oven-ready meals. Also for injection molding applications that call for high flowability.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Viscosity Test 107 cm³/g1.07 dl/gISO 1628
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 250 °C
40 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 130 MPa18900 psiISO 2039-1
Tensile Strength, Yield 57.0 MPa8270 psiISO 527
Elongation at Break 35 %35 %ISO 527
Elongation at Yield 3.7 %3.7 %ISO 527
Tensile Modulus 2.50 GPa363 ksiISO 527
Charpy Impact Unnotched 25.0 J/cm²119 ft-lb/in²ISO 179
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
Tensile Creep Modulus, 1000 hours 11000 MPa1.60e+6 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  3.3
@Frequency 100 Hz
3.3
@Frequency 100 Hz
IEC 60250
 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor  0.0013
@Frequency 100 Hz
0.0013
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 500 V500 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 165 °C329 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75
 
Processing PropertiesMetricEnglishComments
Zone 1 260 - 265 °C500 - 509 °F
Zone 2 265 - 275 °C509 - 527 °F
Zone 3 260 - 270 °C500 - 518 °F
Zone 4 255 - 265 °C491 - 509 °F
Die Temperature 260 - 270 °C500 - 518 °F
Melt Temperature 260 - 270 °C500 - 518 °F
Head Temperature 260 - 270 °C500 - 518 °F
Drying Temperature 100 - 120 °C
@Time 14400 sec
212 - 248 °F
@Time 4.00 hour
Moisture Content <= 0.040 %<= 0.040 %
Precipitation Temperature 260 - 270 °C500 - 518 °F
 
Descriptive Properties
Compression Ratio3.5:1 to 4:1
L/D Ratio25:1 minimum
Three section screw6D/7D/9D + 3D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8902 / 254860

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.