Description: LUTENE XL2808BK has an excellent electrical properties and assists in obtaining a minimum shrink back on aluminum conductor, especially solid conductor. LUTENE XL2808BK is specifically developed to provide a super smooth surface yielding a more perfect interface between the extruded shield and the insulation. LUTENE XL2808BK has stable volume resistivity characteristics at elevated temperatures and is formulated with a polymer system that has demonstrated compatibility with copper conductor. Applications: Insulation shielding of medium and high voltage cable Information provided by LG Chemical |