Applications: AMPCOLOY 95 finds its own applications due to its slightly higher mechanical properties. AMPCOLOY 95 is principally used for spot welding electrodes, electrodes for mesh welding, electrode holders and seam welding discs for stainless steel, Monel and nickel alloys, flash welding dies, plunger tips in aluminum high pressure die casting machines and parts for injection moulding of plastic wherever a high thermal conductivity is desirable. |
CDA C17500; RWMA Class 3; ISO NFA 82100; EN CW 103C Typ A3/1; DIN 17666 W. Nr. 2.1285; AFNOR UK2Be |