MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 78 E 4588 Polyester-Based TPU-High Performance Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: High Hydrolysis resistance and good crystallinity. Suggested for injection molding.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage 0.016 in/inASTM D995
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Hardness, Shore D 30ASTM D2240
Tensile Strength at Break 50.0 MPaDIN 53504
Elongation at Break 730 %ASTM D412
100% Modulus 0.00430 GPa
@Strain 100 %
DIN 53504
300% Modulus 0.00810 GPa
@Strain 300 %
DIN 53504
Rebound 48 %Bayshore; ASTM D2632
Tear Strength 500 pliASTM D624
Abrasion 25[mm3]; ISO 4649
Compression Set 30 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 40 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 175 °CHuntsman/TMA
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not reported

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether
Covestro Desmopan® 5377A Polyurethane
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether

PHU9902 / 150362

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.