MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Petropol Makropol® B3 MF UV CRLA010 PC306 PC, 50% RH
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded; Polycarbonate, Molded

Material Notes: Product Description: Low Viscosity, UV Stabilized, Transparent Color, Polycarbonate

Resin ID (ISO 1043): PC
Additive: UV Resistant
Processing: Injection Molding; Extrusion
Color: Transparent

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 0.12 %0.12 %Equilibrium; ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 66.0 MPa9570 psi50 mm/min; ISO 527-1/-2
Elongation at Break 120 %120 %50 mm/min; ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 98.0 MPa14200 psi2 mm/min; ISO 178
Flexural Modulus 2.35 GPa341 ksi2 mm/min; ISO 178
Flexural Strain at Break 7.0 %7.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 75.0 kJ/m²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature -60.0 °C
NB
@Temperature -76.0 °F
ISO 179-1eU
Charpy Impact, Notched  1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 34.0 kV/mm
@Thickness 1.00 mm
864 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.00050
@Frequency 100 Hz
0.00050
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Melting Point 280 °C536 °FISO 294
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 124 °C255 °FISO 75-1,-2
Vicat Softening Point  144 °C
@Load 5.10 kg
291 °F
@Load 11.2 lb
120 °C/h; ISO 306
 145 °C
@Load 5.10 kg
293 °F
@Load 11.2 lb
50 °C/h; ISO 306
Flammability, UL94  V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 2.60 mm
V-2
@Thickness 0.102 in
Glow Wire Test  850 °C
@Thickness 1.00 mm
1560 °F
@Thickness 0.0394 in
IEC 60695-2-12
 850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
IEC 60695-2-12
 850 °C
@Thickness 2.00 mm
1560 °F
@Thickness 0.0787 in
IEC 60695-2-12
 930 °C
@Thickness 3.00 mm
1710 °F
@Thickness 0.118 in
IEC 60695-2-12
 960 °C
@Thickness 4.00 mm
1760 °F
@Thickness 0.157 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 290 °C518 - 554 °FMolding
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 120 °C248 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL054 / 312962

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.