MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyChem Alloy 6004 Talc Nucleator
Categories: Polymer

Material Notes: Talc nucleator products are additive masterbatch concentrates designed for the nucleation of both commodity and engineering thermoplastic resins. Talc Nucleators typically contain 40 to 60 % by weight of talc in a PE, PP, or PS carrier. Other carriers, and other talc levels, such as 25%, are available upon request. About 80% of the talc particle size used in these products is less than 1 micron, with the remaining particle sizes ranging from 1 to 5 microns. Talc Nucleators are typically used as physical nucleating agents for extruded foam, and are generally used at a 0.4 to 2.0% let-down level, depending upon the application. These products are available in a uniform pellet shape, eliminating the processing concerns associated with dusts or powders.

Key Words: PolyChem Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 1.0 µm1.0 µmat 80% distribution <1 to 5 microns.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 220 °C338 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Noble Polymers Regis™ 115090 Thermoplastic Olefin (TPO)
Chevron Phillips Marlex® EHM 6004 High Density Polyethylene, Blow Molding
Noble Polymers Regis™ 275107 Thermoplastic Olefin (TPO)
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO)
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO)

PPC530 / 56100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.