Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous. The unpigmented material has a light inherent color. RoHS: Grilon TS V0 is in compliance with RoHS (2002/95/EC, Restriction of hazardous Substances). WEEE: Parts produced from Grilon TS V0 are not subject to “selective treatment” according the Directive 2002/96/EC on Waste Electrical and Electronic Equipment. Grilon TS V0 has the following important properties: - halogen free and free of red phosphorous.
- UL-94 V0 at 0.4 mm wall thickness
- High toughness
- Suitable for molded Integral hinges
Grilon TS V0 is used typically for fuses, strips, cable binders, print terminals and coil former bobbins.Information provided by EMS Grivory. |