MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resinlab® AR 1018 Conformal Coating  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Resinlab™ AR 1018 is a one-part low viscosity acrylic based conformal coating for electronic circuit boards. It possesses excellent flexibility and adhesion to many substrates. It provides excellent protection against water, humidity, salt spray and other chemicals. It also contains a fluorescent dye to act as a tracing aid to assure complete coverage and for dropper bottle repair/touch-up.

AR 1018 will dry to the touch in 10 to 15 minutes at 25°C and 50% R.H. and reach through dry in 24 hours. A force dry of 80°C for 30 minutes can be used to accelerate production.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/cc
Solids Content 35 %
Viscosity 150 cP
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.6
Dielectric Strength 7700 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorClear (fluorescent)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM)
Dow SiLK™ D Semiconductor Dielectric Resin
AISI 1018 Steel, cold drawn

PRESL001 / 101415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.