MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent environmental resistance. Excellent for bonding many metals, woods, rubbers and some plastics.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 300000 - 1.00e+6 cP
 70000 - 6.00e+6 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 85
Tensile Strength, Ultimate 4290 psi
Elongation at Break 2.0 - 3.0 %
Modulus of Elasticity 344 ksi
Shear Strength 1100 psiCRS Overlap, White Gas @ RT
 1950 psiCRS Overlap, Tap Water at RT
 2000 - 2200 psiCRS Overlap
 2200 psiCRS Overlap, 100% RH at 49°C
 2250 psiCRS Overlap, Hydraulic Oil at RT
 500 psi
@Temperature 82.0 °C
Aluminum Overlap; ASTM D1002
 1500 psi
@Temperature -55.0 °C
Aluminum Overlap; ASTM D1002
 3000 psi
@Temperature 24.0 °C
Aluminum Overlap; ASTM D1002
Peel Strength 2.00 pli
@Temperature -55.0 °C
Aluminum T-Peel; ASTM D1876
 4.00 pli
@Temperature 24.0 °C
Aluminum T-Peel; ASTM D1876
 4.00 pli
@Temperature 82.0 °C
Aluminum T-Peel; ASTM D1876
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+15 ohm-cm
Dielectric Constant 6.06
@Frequency 1000 Hz
Dielectric Strength 585 kV/in
Dissipation Factor 0.012
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 79.0 µm/m-°C
@Temperature 0.000 - 40.0 °C
Thermal Conductivity 2.03 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 55.0 °C
 
Descriptive Properties
AppearanceGreenAccelerator
 Green
 WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34625 / 169372

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.