MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Danquinsa DANCOLOR® MB-9005/SM Color master batch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCOLOR® MB-9005/SM is a combined masterbatch based on TPU, which is delivered in form of black pigmented granules (pellets). This TPU concentrate is used for black pigmenting of thermoplastic polyurethanes as well as demoulding additive. DANCOLOR® MB-9005/SM can be added to our polyurethanes based on polyester, polycaprolactone as well as to our polyurethanes based on polyether. DANCOLOR® MB-9005/SM is suitable for the processing by extrusion, injection moulding and for melt-calendering.

Application: DANCOLOR® MB-9005/SM can be applied and mixed with all products out of our PEARLTHANE®- or PEARLCOAT®- range ( based on polyester or polyether ) which find their application by extrusion, injection moulding or calandering. This additive is applied everywhere where the parts must be colored into black color acc. to RAL 9005. In addition this combined masterbatch fulfils a better geometry at the demoulding. So it acts also as demoulding additive. In general it are recommended dosages of 1 to 3% ( calculated by the weight of the TPU ) is recommended. Higher doses for the improvement of the demoulding can be also considered but this must be proved before.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³ASTM D1875
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 °C464 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hour
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Color index no.RAL 9005/SM
Composition0.4Carbon pigments
Light fastness8(1-8) blue scale, DIN 53 389

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ050 / 294470

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.