MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tosoh ESL-1 Optical Silica Glass
Categories: Ceramic; Glass

Material Notes: ES ingots are manufactured from high-purity SiCl4 using an oxy-hydrogen flame in a verneuil type process. For very large parts, such as LCD photomasks, ES ingots are reflown into large rectangular blocks. ES ingots have a typical purity that exceeds the detection limit of 10ppb in all elements, and are virtually free of bubbles and inclusions. As a result, ES is the material of choice for LCD photomasks up to Gen. 10, and selected subgrades are widely used in leading edge stepper (KrF and ArF) and optics applications.

Features: Standard optical grade for planar optics

Application: : LCD Mask, Mirror & window substrate

Information provided by Tosh Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³
Viscosity 11400 cP
@Temperature 1200 °C
11400 cP
@Temperature 2190 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 907.5907.5
Tensile Strength 49.0 MPa7110 psi
Modulus of Elasticity 74.0 GPa10700 ksiYoung's
Flexural Strength 65.0 - 95.0 MPa9430 - 13800 psi
Compressive Strength 1130 MPa164000 psi
Poissons Ratio 0.180.18
Shear Modulus 31.0 GPa4500 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cm
Surface Resistance 5.00e+15 ohm5.00e+15 ohm
Dielectric Constant 3.9
@Frequency 5.00e+8 Hz
3.9
@Frequency 5.00e+8 Hz
Dielectric Loss Index <= 0.0010
@Frequency 5.00e+8 Hz
<= 0.0010
@Frequency 5.00e+8 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.520 µm/m-°C
@Temperature 30.0 - 100 °C
0.289 µin/in-°F
@Temperature 86.0 - 212 °F
 0.580 µm/m-°C
@Temperature 30.0 - 200 °C
0.322 µin/in-°F
@Temperature 86.0 - 392 °F
Specific Heat Capacity 0.749 J/g-°C0.179 BTU/lb-°F
Thermal Conductivity 1.38 W/m-K9.58 BTU-in/hr-ft²-°F
Softening Point 1720 °C3130 °F(?=10^7.6)*2
Annealing Point 1080 °C1980 °F(?=10^13)
Strain Point 980 °C1800 °F(?=10^14.5)
 
Descriptive Properties
Applicable Wavelength180-2100 nm
Bubble ClassClass O
Refractive Index Homogeneity3-10CA:F300mm
 5-15CA:F500mm
Strain1-10 nm/cm
Striae1 direction free

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTOSOH017 / 306472

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.