Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity. Applications: Electric, electronic and business machine components that need flame retardance and transparencySlightly thin wall or large moldingsInformation provided by Teijin Chemicals Ltd. |