MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QGel 910 High Refractive Index Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QGel 910 is a clear, very soft, tough, moderately cross-linked, silicone polymeric elastomer, offering exceptional clarity for optical transmission applications. This gel also provides self-healing protection to sensitive devices isolating them from shock, vibration and CTE stress. This particular silicone gel also provides excellent moisture protection and equally outstanding electrical properties over a broad temperature range.

Key Features:

  • One to one mix ratio
  • Soft, but resilient gel
  • Dispensing equipment not necessary
  • Good adhesion with QSil Primer #5

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccUncatalyzed B
 1.05 g/ccUncatalyzed A
Viscosity 400 cPUncatalyzed B
 500 cPUncatalyzed A
 
Mechanical PropertiesOriginal ValueComments
Penetration 2.0 - 6.0
@Temperature 150 °C,
Time 1800 sec
[mm], Cured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 240 °C
Minimum Service Temperature, Air -40.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.463
@Temperature 45.0 °C
 1.468
@Temperature 30.0 °C
 1.475
@Temperature 15.0 °C
 1.47
@Wavelength 589 nm
Transmission, Visible 94.26 %
@Wavelength 400 nm
 95.9 %
@Wavelength 450 nm
 96.5 %
@Wavelength 500 nm
 96.9 %
@Wavelength 745 nm
 97.25 %
@Wavelength 600 nm
 97.56 %
@Wavelength 700 nm
 97.7 %
@Wavelength 750 nm
 97.8 %
@Wavelength 800 nm
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
 30.0 min
@Temperature 150 °C
 60.0 min
@Temperature 100 °C
Gel Time 120 minCatalyzed
 
Descriptive Properties
ColorTransparentUncatalyzed A
 TransparentUncatalyzed B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QGel 319 Optically Clear Silicone Gel
CHT Group QGel 314 General Purpose Silicone Gel
Overview of materials for Silicone Rubber
CHT Group QGel 317 General Purpose Silicone Gel
CHT Group QGel 315 QSI Quantum Silicones General Purpose Silicone Gel

PACC2030 / 199418

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.