MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Makrolon® XT5010 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: MVR (300 °C/1.2 kg) 34 cm³/10 min; easy processing; low viscosity; easy release; vicat softening temperature 50 N; 50 °C/h = 110 °C; injection molding - melt temperature 240 - 280 °C; available in transparent colors only; LCD tv frame

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183-1
Melt Flow 41.14 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 75.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %Nominal, 50 mm/min; ISO 527-1,-2
 90 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 5.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2700 MPa1 mm/min; ISO 527-1,-2
Charpy Impact Unnotched 220 kJ/m²
@Temperature 23.0 °C
complete break; ISO 179-1eU
 NB
@Temperature -30.0 °C
ISO 179-1eU
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 112 °C
@Load 5.10 kg
50°C/h; ISO 306
 114 °C
@Load 5.10 kg
120°C/h; ISO 306
UL RTI, Electrical 80.0 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical with Impact 80.0 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical without Impact 80.0 °C
@Thickness 1.50 mm
UL 746B
Flammability, UL94 V-2
Glow Wire Ignition Temperature 800 °C
@Thickness 0.750 mm
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.750 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection molding; ISO 294
Mold Temperature 80.0 °CInjection molding; ISO 294
Injection Velocity 200 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2256 Polycarbonate
Covestro Makrolon® 2665 Polycarbonate
Covestro Makrolon® 2667 Polycarbonate
Covestro Makrolon® ET2613 Polycarbonate
Covestro Makrolon® ET3117 Polycarbonate

PB09652 / 150784

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.