MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Polystone® G natural PE-HD
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product characteristics:
  • Very good welding and processing properties
  • Good chemical resistance
  • High adhesion in a composite system and so highly suitable for tank building
Product applications:
  • Chemical engineering and tank building
  • Corrosion protection

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccDIN EN ISO 1183-1
Water Absorption <= 0.010 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63DIN EN ISO 868
Tensile Strength, Yield 22.0 MPaDIN EN ISO 527
Elongation at Break >= 50 %DIN EN ISO 527
Modulus of Elasticity 0.800 GPaDIN EN ISO 527
Izod Impact, Notched (ISO) 12.0 kJ/m²DIN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+14 ohmDIN EN 62631-3-2
Dielectric Constant 2.4IEC 60250
Dielectric Strength 45.0 kV/mmIEC 60243
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 - 230 µm/m-°CDIN 53752
Specific Heat Capacity 1.90 J/g-°CDIN 52612
Thermal Conductivity 0.400 W/m-KDIN 52612-1
Melting Point 135 °CISO 11357-3
Maximum Service Temperature, Air 80.0 °Clong term
 100 °Cshort term
Vicat Softening Point 67.0 °CDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air -50.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 HB
@Thickness 6.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake EC850AA Low Density Polyethylene
LyondellBasell Petrothene® NA217080 Low Density Polyethylene
Borealis FA6220 Low Density Polyethylene

PROCH9218 / 232921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.