MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crosspolimeri GETILAN MAC/900 R Crosslinkable Polyolefinic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: GETILAN: is the trade-mark of our crosslinkabe (SIOPLAS technology) polyolefinic compounds

GETILAN MAC/900 R: this semiconductive product , HEPR base, crosslink by osmosis using them together with our types POLIGOM G/...or GETILAN GPE/.... It do not soil the copper. When the material is extruded in contact with the red copper conductor, the -SCU type must be used

Certify: Internal Semiconductive Crosslinkable

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D792
Melt Flow 1.0 - 6.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
1.0 - 6.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 10.0 MPa>= 1450 psiIEC 60811
Elongation at Break >= 300 %>= 300 %IEC 60811
 >= 100 %
@Temperature 135 °C,
Time 605000 sec
>= 100 %
@Temperature 275 °F,
Time 168 hour
Crosslinked Specimens; IEC 60811
 
Processing PropertiesMetricEnglishComments
Zone 1 140 °C284 °F
Zone 2 150 °C302 °F
Zone 3 160 °C320 °F
Zone 4 170 °C338 °F
Die Temperature 190 °C374 °F
Head Temperature 185 °C365 °F
Dry Time  60.0 hour
@Temperature 6.00 °C
60.0 hour
@Temperature 42.8 °F
 70.0 hour
@Temperature 10.0 °C
70.0 hour
@Temperature 50.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS123 / 294207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.