Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the following important properties:- Very high melt strength
- Very high flexibility
- Excellent toughness at low temperatures
- Processable on conventional as well as on 3 D-machines
- Suitable for sequential blow molding technology
Grilon ELX 50 H NZ is used typically as flexible part in the sequential blow molding technology in combination with a rigid PA6 grade such as Grilon EB 50 H or Grilon R 50 H NZ or Grilon EBV-15H. Application examples are air ducts for turbo-chargers and engine air ducts.Information provided by EMS Grivory. |