MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® C33 L PA6/66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Description: Ultramid® C33 L is a lubricated copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Ultramid® C33 L is well suited for the production of nonsymmetric blown film with reduced curl. Its lower melting point than standard PA 6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. Product supplied in 2-2.5 mm round pellets.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.690 - 0.710 g/cc
Density 1.12 g/ccISO 1183
Moisture Absorption at Equilibrium 3.2 %23°C/50% RH
Water Absorption at Saturation 10.5 %23°C
Viscosity Measurement 3.19 - 3.41(RV) 1% [m/v] in 96% [m/m] sulfuric acid; ISO 307
 187 - 203(RV) 0.5% [m/v] in 96% [m/m] sulfuric acid; ISO 307
 
Thermal PropertiesOriginal ValueComments
Melting Point 195 - 197 °CISO 3146
Decomposition Temperature >= 300 °C
Ignition Temperature >= 400 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.080 %ISO 15512
 
Descriptive Properties
Commercial StatusEurope
Extractables<0.8 %ISO 6427
Film Grade1-3BASF
Lubricant250 - 550 mg/kgBASF

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B33LN 01 PA6 (Dry)
BASF Ultramid® B40LN 01 PA6 (Dry)
BASF Ultramid® B36 LN 01 PA6
BASF Ultramid® C40 L 01 PA6/66
BASF Ultramid® C33 PA6/66

PBASG0408 / 132041

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.