MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Saint-Gobain Furon® C695 Thermal Graphite Tape
Categories: Carbon; Graphite; Polymer; Adhesive; Tape

Material Notes: A 5 mil flexible graphite film coated on one side with 1 mil thickness of thermally-conductive acrylic pressure-sensitive adhesive. Recommended uses: One-sided adhesive allows for easy rework and upgrades. The heat spreading capabilities make it ideal for use with multiple components using one heat sink. Application advantages: Graphite film spreads heat evenly to allow for maximum heat sink potential at low pressures; Only pressure sensitive graphite tape available in the world; One-sided adhesive construction allows for easy rework, replacement, or upgrade of components; Pressure-sensitive adhesive tape can be pre-applied to a heat sink to minimize assembly costs; Flame-retardant version available; Available in slit-rolls or die-cut shapes. All data based on a 0.006 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 500 psiASTM D1000
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 4.00 W/m-KASTM E1530
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -20.0 °F
 
Descriptive Properties
ColorMetallic Black
Thermal Impedance @ 10 psi0.10°C in^2/WASTM E1530

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
96% Alumina, thick-film, as fired
3M 6Ns Ultra High Purity Boron
Avient Polystrand ThermoPro™ IE7020 Unitape Unidirectional Polyethylene-Glass Composite
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Poco Graphite EDM-AF5 EDM Graphite

PSTGQZ477 / 68991

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.