MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chi Mei Polylac® PA-746Y ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Medium flow, high impact

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Melt Flow 15 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 101 MPaH358/30; ISO 2039-1
Tensile Strength at Break 35.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 47.0 MPa50 mm/min; ISO 527
Elongation at Break 15 %50 mm/min; ISO 527
Flexural Strength 65.0 MPa2 mm/min; ISO 178
Flexural Modulus 2.00 GPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 23.0 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) NBISO 180/1C
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 2.60 J/cm²ISO 179
Impact 17Impact Flexural Test Notched (KJ/m²)
 NBImpact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °Cunannealed; ISO 75
 99.0 °Cannealed; ISO 75
Vicat Softening Point 98.0 °C
@Load 5.00 kg
50°C/hr; ISO 306
 98.0 °C
@Load 5.00 kg
120°C/hr; ISO 306
 104 °C
@Load 1.00 kg
50°C/hr; ISO 306
 106 °C
@Load 1.00 kg
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
UL 94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Covestro Bayblend® T65 HI PC/ABS Blend
Covestro Makrolon® 2405 MAS048 Polycarbonate
Covestro Makrolon® 2407 Polycarbonate, Injection Grade

PCHI914 / 109402

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.