MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Aptek 2205 A/B Low modulus urethane stacking compound
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: APTEK 2205-A/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although APTEK 2205-A/B is capable of achieving full cure at room temperature, a short term exposure to moderate heat will greatly reduce processing time and optimize cured properties.

Good wet strength holds components in place allowing for the movement of the circuit boards during processing; 100% solids, solvent free system that will not form voids during cure or service life; Low Tg for excellent low-temperature cycling and performance; Very good substrate adhesion, superior to silicones; Available at two levels of reactivity to meet various productivity needs; available in pre-weighted kits to minimize handling time; ideal for field repair operations

APTEK 2205-A is a filled polyol resin that is safe to handle when used properly.. APTEK 2205-B is an organic isocyanate which make cause severe eye and skin irritation with direct contact..

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccA Component; ASTM D1475
 1.21 g/ccB Component; ASTM D1475
Viscosity 88 cPB Component; ASTM D1824
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65Cured property; ASTM D2240
Tensile Strength, Ultimate 875 psiCured property; ASTM D412
Elongation at Break 265 %Cured property; ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.30e+15 ohm-cmCured property; ASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
Cured property; ASTM D150
Dissipation Factor 0.030
@Frequency 1000 Hz
Cured property; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 79.0 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 1; JMTP P200
 185 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 2; JMTP P200
Glass Transition Temp, Tg -70.0 °CCured property; JMTP P-200
Flash Point >= 125 °CB Component; ASTM D92
 >= 150 °CA Component; ASTM D92
 
Processing PropertiesOriginal ValueComments
Processing Temperature 85.0 °CCure 4 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DSM Biomedical Bionate® 75D Thermoplastic Polycarbonate Polyurethane (PCU)
3D Systems QuickPlastic Cast Urethane Material PELike 70 A
AK Steel 2205 Duplex Stainless steel
Carlson 2205 (UNS S32205) Duplex Stainless Steel
Indium Corp. 2205 Rosin Flux

PAPTEK25 / 24187

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.