MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Malvern Minerals Wollastokup® FF Silane Treated Wollastonite
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Wollastokup® is a custom, silane treated calcium metasilicate (wollastonite) which is used as a functional filler in coatings, plastics, rubber and others due in part to its acicular or “toothpick” shape. Within coatings, Wollastokup® improves the durability of the film, improves resistance to weathering, reduces gloss, acts as a flatting and suspending agent and reduces pigment consumption. In plastics, improvements in tensile and flexural strength along with reduction in resin consumption are among the many benefits within plastics. Additionally, improvements in thermal and dimensional stability at elevated temperatures are noted within plastics.

Information provided by Malvern Minerals Company.

Key Words: CaSiO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.90 g/cc2.90 g/cc
Oil Absorption 32 %32 %
Moisture Absorption at Equilibrium <= 0.10 %<= 0.10 %
Particle Size 18 µm18 µmD50
pH 9.0 - 109.0 - 10
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 4.0 - 5.04.0 - 5.0
 
Thermal PropertiesMetricEnglishComments
Melting Point 838 °C1540 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.631.63
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.25 %0.25 %
CaO 46.5 %46.5 %
Fe2O3 0.20 %0.20 %
Loss on Ignition(%) <= 1.0 %<= 1.0 %Inorganic
MgO 0.20 %0.20 %
SiO2 52.2 %52.2 %
 
Descriptive Properties
ColorWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Malvern Minerals Novacite® Daper Untreated Lamellar Quartz Filler/Extender
Imerys ULTRAFIBRE® II Wollastonite
Imerys NYGLOS® 2 Wollastonite
Imerys NYAD® G Special Wollastonite
Imerys 10 AS WOLLASTOCOAT® Wollastonite

CMALV935 / 149114

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.