MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman HT 976 Aromatic Amine
Categories: Polymer; Thermoset; Epoxy

Material Notes: Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.

Comments/Applications: 4,4'-diaminodiphenyl sulfone (DDS). Solid amine with a melting point of 174 - 178°C. Excellent high temperature and chemical resistance. Adhesives, PWB laminates, prepregs, composites.

Data provided by Ciba Specialty Chemicals.

Ciba Specialty Chemicals has been acquired by Huntsman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 174 - 178 °CSoftening Range
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 °CCure Schedule: 4 hrs. at 175°C or 24 hrs at 120°C.
Pot Life 180 min
@Temperature 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman Araldite GY 6010 Bisphenol A Epoxy Liquid Resin
Atom Adhesives AA-BOND F253 Epoxy Adhesive
Huntsman HT 9664 Aromatic Amine
Elantas Conap FR-1200 / EA-117 Conapoxy® Resin / Conacure® Hardener
Elantas Conap FR-1080 Conapoxy® Resin / Conacure® Hardener

PCIC45 / 28544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.